MIG soude fil pou asye pur ER317 presyon aparèy chofaj soude machandiz yo


TEKNOLOJI soude
Pa kite kesyon yo
Kontinye ante ou

Arc enstabilite

Bòdi disgrasyeu

Twòp sal
Metal la fusion gen bon mekanik
pwopriyete ak ekselan rezistans korozyon
Segondè estrikti rezistans korozyon tankou 0Cr19Ni13Mo3 (SUS317),
souvan itilize nan angrè ak pwodiksyon ure oswa ekipman depo.

Ripple byen
Lis fil manje, arc ki estab, bèl fòme
Bon likidite nan fè fonn, mwens Splash ak ekselan pèfòmans pwosesis soude.

Fasil salop
Paramèt pwodwi
KONPONÈ CHIMIK:
ALLOY (poids%) | C | Mn | Si | P | S | Ni | Cr | Mo | Lòt |
RÈG GB/T | 0.018 | 0.51 | 1.72 | 0.016 | 0.005 | 13.48 | 19.08 | 3.23 | - |
PWOPRIYETE MEKANIK:
PWOPRIYETE | FÒS RENDE (MPa) | FÒS ekstansyon (MPa) | elongasyon/% | VALÈ IMAPACT J/℃ | Tretman chalè °C*h | |||||
RÈG GB/T | - | 565 | 43 | - | - |
PARAMÈT SOUDE REKÒMANDE:
DYAMET SPECIFICATIONS (mm) | 0.8 | 1.0 | 1.2 | ||||
ELEKTRISITE (Amp) | H/W | 70-150 | 100-200 | 140-220 | |||
O/W | 50-120 | 80-150 | 120-180 |
Sipò faktori




Pwodwi a apwopriye pou yon
pakèt aplikasyon
TEKNOLOJI soude

Entèn raktor

-
981 semi-submersible forage mare

-
8.2-tòn transpòtè esansyèl
KONPONÈ CHIMIK:
ALLOY (poids%) | C | Mn | Si | P | S | Ni | Cr | Mo | Lòt |
RÈG GB/T | 0.018 | 0.51 | 1.72 | 0.016 | 0.005 | 13.48 | 19.08 | 3.23 | - |
PWOPRIYETE MEKANIK:
PWOPRIYETE | FÒS RENDE (MPa) | FÒS ekstansyon (MPa) | elongasyon/% | VALÈ IMAPACT J/℃ | Tretman chalè °C*h | |||||
RÈG GB/T | - | 565 | 43 | - | - |
PARAMÈT SOUDE REKÒMANDE:
DYAMET SPECIFICATIONS (mm) | 0.8 | 1.0 | 1.2 | ||||
ELEKTRISITE (Amp) | H/W | 70-150 | 100-200 | 140-220 | |||
O/W | 50-120 | 80-150 | 120-180 |